Alloy Grade UNS: CAF 765 – Stainless Steel Alloy

  • Overview

    CAF 765 is a specialized stainless steel alloy engineered to withstand demanding high-temperature environments. This heat-resistant alloy maintains its strength and structural integrity at elevated temperatures, making it suitable for applications where components are exposed to extreme heat and thermal cycling. CAF 765 resists oxidation and creep, phenomena that can degrade materials at high temperatures, ensuring long-term performance and reliability in demanding conditions. Its ability to withstand heat makes it a valuable choice for applications in industries such as aerospace, power generation, and chemical processing, where components must operate reliably under extreme thermal conditions.

  • Typical Uses

    Petrochemical parts.

  • MetalTek Grade

    CAF 765

  • Poured At:

    Carondelet Division, Sandusky International Division, Wisconsin Investcast Division

Similar Specifications

Typical Chemical Composition (% by wt.)

Aluminum: n/a

Carbon: 0.45-0.50

Chromium: 25.0-27.5

Manganese: 1 MAX

Iron: BAL

Copper: n/a

Nickel: 34.0-36.5

Lead: n/a

Tin: n/a

Silicon: 1.4-2.0

Zinc: n/a

Other: Co 14-16; W 4.5-5.5

Minimum Mechanical Properties

Tensile, ksi

0

Tensile, MPa

0

Calculated PREn (Minimum)

0

Yield, ksi

0

Yield, MPa

0

Elongation

0%